• Home
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
  • Issues
    • All Issues
    • Recent issue
    • Early views
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Issues

Recent Issue
 

Journal of Ceramic Science and Technology 2/2019

Vol. 10, No. 2

Original Articles

Source:
Journal of Ceramic Science and Technology

The Phase Composition and Mechanical Properties of Al2O3-TiN-TiC Ceramic Materials with Different Ni Content

Y. Fei, Ch. Huang, H. Liu

Vol. 10, No. 2, Pages 1-8   DOI: 10.4416/JCST2019-00012

Keywords: Al2O3-TiN-TiC ceramic, Ni content, phase composition, mechanical properties

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Influence of the Printing Parameters on the Quality of Alumina Ceramics Shaped by UV-LCM Technology

P. Ożóg, G. Blugan, D. Kata, T. Graule

Vol. 10, No. 2, Pages 1-10   DOI: 10.4416/JCST2019-00023

Keywords: Alumina, LCM, 3D printing, UV-curing, photopolymerisation

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Design and Experiment of a 3D Printing System for Ceramics by Continuous Extrusion

Y. CHAO, X. LIU

Vol. 10, No. 2, Pages 1-10   DOI: 10.4416/JCST2019-00048

Keywords: 3D ceramic printing, continuous extrusion, nozzle extrusion device, bonding quality.

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Avoiding Thermal-Stress-Induced Failures by Design Optimization when Brazing Perlucor® to Inconel® 718 Components

L. Spatafora, J. Isele, H.-J. Ritzhaupt-Kleissl, V. Hagenmeyer, J. Aktaa

Vol. 10, No. 2, Pages 1-10   DOI: 10.4416/JCST2019-00011

Keywords: Metal-ceramic-joint, residual stress calculation, failure probability, active brazing

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Effect of the Evolution of Rheological Behavior over Deagglomeration Time on Optical Transparency of Polycrystalline Alumina Ceramics

A. Rahimian, M. Torki, S. Ghazanfari, B. Movahedi, R. Emadi

Vol. 10, No. 2, Pages 1-8   DOI: 10.4416/JCST2019-00047

Keywords: Optical materials, sintering, optical properties, ball milling.

Abstract  |  References  |  Full Article

Source:
Journal of Ceramic Science and Technology

Low-Temperature Sintering and Microwave Dielectric Properties of Li2O-3ZnO-5TiO2 Ceramics Doped with B2O3

J. Liu, J. Zhu, Y. Zeng

Vol. 10, No. 2, Pages 1-8   DOI: 10.4416/JCST2019-00055

Keywords: Microwave dielectric properties, LTCC, Li2O-3ZnO-5TiO2

Abstract  |  References  |  Full Article

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH