• Home
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Effect of Conventional and Rapid Sintering on the Mechanical and Hydrothermal Aging Properties of 5Y-TZP Dental Zirconia

Yena Jang, Jae Chul Bang

Department of Materials Science and Engineering, Soonchunhyang University, 646 Eupnaeri, Asan, Chungnam 31538, Republic of Korea

received November 27, 2025, received in revised form February 4, 2026, accepted February 10, 2026

Pages 1-10   DOI: 10.4416/JCST2025-00016

Abstract

This study investigated the effects of sintering methods on the mechanical properties and hydrothermal aging resistance of 5 mol% yttria-stabilized tetragonal zirconia polycrystals (5Y-TZP), a material widely used for dental restorations due to its aesthetic translucency. Specimens were fabricated using both conventional sintering (CS) and rapid sintering (RS) at two temperatures (1 450 °C and 1 600 °C), and their flexural strength, fracture toughness, and Vickers hardness were compared. X-ray diffraction (XRD) and SEM analyses confirmed that all sintered specimens exhibited dense microstructures with no monoclinic phase detected even after low-temperature degradation (LTD) testing for up to 20 h. CS specimens consistently demonstrated superior mechanical properties, particularly in fracture toughness and flexural strength, and exhibited higher reliability based on Weibull analysis. While RS offered shorter processing times, it showed slightly inferior mechanical properties. The results indicate that, although both sintering methods produced LTD-resistant 5Y-TZP, optimizing the RS parameters is necessary to bridge the performance gap with CS, especially for long-span prosthetic applications.

Download Full Article (PDF)

Keywords

Yttria-stabilized tetragonal zirconia polycrystals, rapid sintering, conventional sintering, low-temperature degradation, flexural strength, Weibull analysis

References

1 Picconi, C., Maccauro, G.: Zirconia as a ceramic biomaterial, Biomaterials, 20, 1 – 25, (1999).

2 Denry, I., Kelly, J.R.: State of the art of zirconia for dental applications, Dent. Mater., 24, 299 – 307, (2008).

3 Miyazaki, T., Nakamura, T., Matsumura, H., Ban, S., Kobayashi, T.: Current status of zirconia restoration, J. Prosthodont. Res., 57, 236 – 261, (2013).

4 Jansen, J.U., Lümkemann, N., Letz, I., Pfefferle, R., Sener, B., Stawarczyk, B.: Impact of high-speed sintering on translucency, phase content, grain sizes, and flexural strength of 3Y-TZP and 4Y-TZP zirconia materials, J. Prosthet. Dent., 122, 396 – 403, (2019).

5 Kosmač, T., Oblak, C., Jevnikar, P., Funduk, N., Marion, L.: The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic, Dent. Mater., 15, 426 – 433, (1999).

6 Zhang, F., Vanmeensel, K., Batuk, M., Hadermann, J., Inokoshi, M., Van Meerbeek, B., Naert, I., Vleugels, J.: Highly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation, Acta Biomater., 16, 215 – 222, (2015).

7 Studart, A.R., Filser, F., Kocher, P., Gauckler, L.J.: In vitro lifetime of dental ceramics under cyclic loading in water, Biomaterials, 28, 2695 – 2705, (2007).

8 Zhang, Y., Kim, J.W.: Graded zirconia glass for resistance to veneer fracture, J. Dent. Res., 89, 1057 – 1062, (2010).

9 Elias, C.N., dos Santos, H.E.S., Garbossa, M., dos Santos, C.: Mechanical properties of zirconia Y-TZP core veneered for dentistry applications, J. Ceram. Sci. Technol., 8, 525 – 530, (2017).

10 Carrabba, M., Keeling, A.J., Aziz, A., Vichi, A., Fonzi, R.F., Wood, D., Ferrari, M.: Translucent zirconia in the ceramic scenario for monolithic restorations: A flexural strength and translucency comparison test, J. Dent., 60, 70 – 76, (2017).

11 Lawson, N.C., Maharishi, A.: Strength and translucency of zirconia after high-speed sintering, J. Esthet. Restor. Dent., 32, 219 – 225, (2020).

12 Li, L., Zhao, C., Du, Z., Qiu, Y., Si, W.: Rapid-sintered dental zirconia for chair-side one-visit application, Int. J. Appl. Ceram. Technol., 16, 1830 – 1835, (2019).

13 Čokić, S.M., Cóndor, M., Vleugels, J., Van Meerbeek, B., Van Oosterwyck, H., Inokoshi, M.: Mechanical properties, aging stability and translucency of speed-sintered zirconia for chairside restorations, Dent. Mater., 36, 959 – 972, (2020).

14 Lubauer, J., Schuenemann, F.H., Belli, R., Lohbauer, U.: Speed-sintering and the mechanical properties of 3 – 5 mol% Y2O3-stabilized zirconias, Odontology, 111, 883 – 890, (2023).

15 Kaizer, M.R., Gierthmuehlen, P.C., dos Santos, M.B.F., Cava, S.S., Zhang, Y.: Speed sintering translucent zirconia for chairside one-visit dental restorations: optical, mechanical, and wear characteristics, Ceram. Int., 43, 10999 – 11005, (2017).

16 Too, T.D.C., Inokoshi, M., Nozaki, K., Shimizubata, M., Nakai, H., Liu, H., Minakuchi, S.: Influence of sintering conditions on translucency, biaxial flexural strength, microstructure, and low-temperature degradation of highly translucent dental zirconia, Dent. Mater. J., 40, 1320 – 1328, (2021).

17 Kongkiatkamon, S., Peampring, C.: Effect of speed sintering on low temperature degradation and biaxial flexural strength of 5Y-TZP zirconia, Molecules, 27, 5272, (2022).

18 Chevalier, J.: What future for zirconia as a biomaterial?, Biomaterials, 27, 535 – 543, (2006).

19 Yoshimura, M., Noma, T., Kawabata, K., Sōmiya, S.: Role of H2O on the degradation process of Y-TZP. In: Hydrothermal Reactions for Materials Science and Engineering. Springer, Dordrecht, 396 – 398, (1989).

20 Hjerppe, J., Özcan, M.: Zirconia: more and more translucent, Curr. Oral Health Rep., 10, 203 – 211, (2023).

21 Swab, J.J.: Low temperature degradation of Y-TZP materials, J. Mater. Sci., 26, 6706 – 6714, (1991).

22 Chevalier, J., Calès, B., Drouin, J.M.: Low-temperature aging of Y-TZP ceramics, J. Am. Ceram. Soc., 82, 2150 – 2154, (1999).

23 Deville, S., Chevalier, J.: Martensitic relief observation by atomic force microscopy in yttria-stabilized zirconia, J. Am. Ceram. Soc., 86, 2225 – 2227, (2003).

24 Lilley, E.: Review of low temperature degradation in Y-TZP's. In: narayan, R. (Ed.), Corrosion and Corrosive Degradation of Ceramics. Woodhead Publishing, Cambridge, 387 – 407, (1990).

25 Lawson, S.: Environmental degradation of zirconia ceramics, J. Eur. Ceram. Soc., 15, 485 – 502, (1995).

26 Deville, S., Chevalier, J., Fantozzi, G., Bartolomé, J.F., Requena, J., Moya, J.S., Torrecillas, R., Díaz, L.A.: Low-temperature ageing of zirconia-toughened alumina ceramics and its implication in biomedical implants, J. Eur. Ceram. Soc., 23, 2975 – 2982, (2003).

27 Yoshimura, M.: Phase stability of zirconia, Am. Ceram. Soc. Bull., 67, 1950 – 1955, (1988).

28 Lughi, V., Sergo, V.: Low temperature degradation -aging- of zirconia: A critical review of the relevant aspects in dentistry, Dent. Mater., 26, 807 – 820, (2010).

29 International Organization for Standardization: ISO 13356:2015 – Implants for surgery — Ceramic materials based on yttria-stabilized tetragonal zirconia (Y-TZP). ISO, Geneva, (2015).

30 Elsherif, R.H., Mandour, M.H., Amin, R.A., El Etreby, A.: Effect of artificial aging on hardness and surface roughness of two types of zirconia, Future Dent. J., 6, 1 – 15, (2020).

31 Pereira, G.K.R., Venturini, A.B., Silvestri, T., Dapieve, K.S., Montagner, A.F., Soares, F.Z.M., Valandro, L.F.: Low-temperature degradation of Y-TZP ceramics: A systematic review and meta-analysis, J. Mech. Behav. Biomed. Mater., 55, 151 – 163, (2016).

32 Chevalier, J., Deville, S., Münch, E., Jullian, R., Lair, F.: Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis, Biomaterials, 25, 5539 – 5545, (2004).

33 Zhang, F., Van Meerbeek, B., Vleugels, J.: Importance of tetragonal phase in high-translucent partially stabilized zirconia for dental restorations, Dent. Mater., 36, 491 – 500, (2020).

34 Pereira, G.K.R., Guilardi, L.F., Dapieve, K.S., Kleverlaan, C.J., Rippe, M.P., Valandro, L.F.: Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations, J. Mech. Behav. Biomed. Mater., 85, 57 – 65, (2018).

35 Kim, J.W., Covel, N.S., Guess, P.C., Rekow, E.D., Zhang, Y.: Concerns of hydrothermal degradation in CAD/CAM zirconia, J. Dent. Res., 89, 91 – 95, (2010).

36 Alves, M.F.R.P., de Campos, L.Q.B., Simba, B.G., da Silva, C.R.M., Strecker, K., dos Santos, C.: Microstructural characteristics of 3Y-TZP ceramics and their effects on the flexural strength, Ceramics, 5, 798 – 813, (2022).

37 Zhang, F., Inokoshi, M., Batuk, M., Hadermann, J., Naert, I., Van Meerbeek, B., Vleugels, J.: Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations, Dent. Mater., 32, 327 – 337, (2016).

38 Alfahed, B., Alayad, A.: The effect of sintering temperature on vickers microhardness and flexural strength of translucent multi-layered zirconia dental materials, Coatings, 13, 688, (2023).

39 Rocha-Rangel, E.: Fracture toughness determinations by means of indentation fracture. In: narayan, R. (Ed.), Nanocomposites with Unique Properties and Applications in Medicine and Industry. Woodhead Publishing, Cambridge, 21 – 38, (2011).

40 Chevalier, J., Gremillard, L., Virkar, A.V., Clarke, D.R.: The tetragonal – monoclinic transformation in zirconia: lessons learned and future trends, J. Am. Ceram. Soc., 92, 1901 – 1920, (2009).

41 Zhang, F., Vanmeensel, K., Inokoshi, M., Batuk, M., Hadermann, J., Van Meerbeek, B., Vleugels, J.: 3Y-TZP ceramics with improved hydrothermal degradation resistance and fracture toughness, J. Eur. Ceram. Soc., 34, 2453 – 2463, (2014).

42 Garvie, R.C., Nicholson, P.S.: Phase analysis in zirconia systems, J. Am. Ceram. Soc., 55, 303 – 305, (1972).

43 Yagli, O.S., Cevlik, E.T., Arpacay, D.K.: The impact of aging and thickness on flexural strength of various zirconia ceramics, BMC Oral Health, 24, 967, (2024).

44 Koenig, V., Wulfman, C.P., Derbanne, M.A., Dupont, N.M., Le Goff, S.O., Tang, M.L., Leforestier, J.F.: Aging of monolithic zirconia dental prostheses: protocol for a 5-year prospective clinical study using analyses, Contemp. Clin. Trials Commun., 4, 25 – 32, (2016).

45 Feighery, A., Irvine, J.T.S.: Effect of alumina additions upon electrical properties of 8 mol.% yttria-stabilised zirconia, Solid State Ionics, 121, 209 – 216, (1999).

46 Ross, I.M., Rainforth, W.M., McComb, D.W., Scott, A.J., Brydson, R.: The role of trace additions of alumina to yttria-tetragonal zirconia polycrystals (Y-TZP), Scr. Mater., 45, 653 – 660, (2001).

47 Kern, F.: 2.75 Yb-TZP ceramics with high strength and ageing resistance. J. Ceram. Sci. Technol., 2, 147 – 153, (2011).

48 Nonaka, K., Teramae, M., Pezzotti, G.: Evaluation of the effect of high-speed sintering and specimen thickness on the properties of 5 mol% yttria-stabilized dental zirconia sintered bodies, Materials, 15, 5685, (2022).

49 Kern, F., Lindner, V., Gadow, R.: Low-temperature degradation behaviour and mechanical properties of a 3Y-TZP manufactured from detonation-synthesized powder, J. Ceram. Sci. Technol., 7, 313 – 322, (2016).

50 Stawarczyk, B., Özcan, M., Hallmann, L., Ender, A., Mehl, A.: The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio, Clin. Oral Investig., 17, 269 – 274, (2013).

51 Kulyk, V.V., Duriagina, Z.A., Vasyliv, B.D., Vavrukh, V.I., Lyutyy, P.Ya., Kovbasiuk, T.M., Holovchuk, M.Ya.: Effects of yttria content and sintering temperature on the microstructure and tendency to brittle fracture of yttria-stabilized zirconia, Arch. Mater. Sci. Eng., 109, 65 – 79, (2021).

52 Kulyk, V., Duriagina, Z., Kostryzhev, A., Vasyliv, B., Marenych, O.: The effect of sintering temperature on the phase composition, microstructure, and mechanical properties of yttria-stabilized zirconia, Materials, 15, 2707, (2022).

53 Inokoshi, M., Zhang, F., De Munck, J., Minakuchi, S., Van Meerbeek, B., Vleugels, J., Naert, I., Vanmeensel, K.: Influence of sintering conditions on low-temperature degradation of dental zirconia, Dent. Mater., 30, 669 – 678, (2014).

54 Chevalier, J., Fantozzi, P., Gremillard, G., Deville, S.: Isothermal sintering effects on phase separation and grain growth in yttria-stabilized tetragonal zirconia polycrystal, J. Eur. Ceram. Soc., 23, 2825 – 2836, (2003).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH