• Home
  • Login
  • Privacy
  • Imprint

Search

Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Effects of B2O3-V2O5 on Sinterability and Microwave Dielectric Properties of (Mg1-xCux)2SiO4 Ceramics

Chengxi Hu, Xiechao Hu, Ze Qing Guo, Amanda Ekeminiabasi Williams

Xihang university, Xi'an, Shaanxi CHINA

received June 3, 2025, received in revised form October 15, 2025, accepted October 16, 2025

Vol. 17, No. 1, Pages 101-106   DOI: 10.4416/JCST2025-00018

Abstract

The crystal structure, microstructure, and microwave dielectric properties of B2O3-V2O5 co-doped (Mg1-xCux)2SiO4 (x=0.05 – 0.20) ceramics were investigated. The sintering temperature was successfully reduced to about 1 250 °C/4 h for the B2O3-V2O5 co-doped (Mg1-xCux)2SiO4 specimens. The (Mg0.95Cu0.05)2SiO4 with 6 wt% B2O3 – 6 wt% V2O5 ceramics sintered at 1 250 °C for 4 h achieved excellent microwave dielectric properties of εr = 6.55, Q·ƒ = 37 500 GHz and a τƒ of - 35.65 ppm/K.

Download Full Article (PDF)

Keywords

Microwave dielectric properties, B2O3-V2O5 co-doped, (Mg0.95Cu0.05)2SiO4, microwave ceramics

References

1 Su, X., Ma, L., Tian, G., et al.: Microwave dielectric properties, chemical bonds and infrared reflection spectra of LiMg6AlO8 ceramics with rock salt structures, J. Eur. Ceram. Soc., 45, [8], 117273 – 117273, (2025). doi: https://doi.org/10.1016/j.jeurceramsoc.2025.117273.

2 Kang, D., Liu, Z., Wen, T., et al.: Crystal structural dependence of microwave dielectric characteristics of novel BaM2N3O10 trisilicate ceramics, J. Alloy. Compd., 1002, 175377 (2024). doi: https://doi.org/10.1016/j.jallcom.2024.175377.

3 Lai, Y., Tang, X., Zhang, H., et al.: Correlation between structure and microwave dielectric properties of low-temperature-fired Mg2SiO4 ceramics, Mat. Res. Bull., 11, 99496 – 502, (2018). doi: https://doi.org/10.1016/j.materresbull.2017.11.036

4 Zhou, X., Xue, G., Su, Y., et al.: Optimized dielectric energy storage performance in ZnO-modified Bi0.5Na0.5TiO3-Sr0.7Bi0.20.1TiO3 ceramics with composite structure and element segregation, Chem. Eng. J., 458, 141449, (2023). DOI number:10.1016/j.cej.2023.141449

5 Hu, C., Liu, Y., Liu, P., et al.: Novel low loss, low permittivity (1-x) SiO2-xTiO2+ ywt% H3BO3 microwave dielectric ceramics for LTCC applications, J. Alloy. Compd., 712, 804 – 810, (2017). doi: https://doi.org/10.1016/j.jallcom.2017.04.079.

6 Hu, C., Liu, P.: Microwave dielectric properties of SiO2 ceramics with addition of Li2TiO3, Mat. Res. Bull., 65, 132 – 136, (2015). doi: https://doi.org/10.1016/j.materresbull.2015.01.034.

7 Rose, A., Masin, B., Sreemoolanadhan, H., et al.: Synthesis and microwave dielectric studies of pure Li2MgSiO4 and B2O3, MgF2, WO3 added Li 2 MgSiO4 for substrate applications, Appl. Surf. Sci., 449, 96 – 104, (2018). doi: https://doi.org/10.1016/J.APSUSC.2018.01.077

8 Lai, Y., Tang, X., Zhang, H., et al.: Correlation between structure and microwave dielectric properties of low-temperature-fired Mg2SiO4 ceramics, Mat. Res. Bull., 99, 496 – 502, (2018). doi: https://doi.org/10.1016/j.materresbull.2017.11.036

9 Tian, H., Liu, Y., Zhang, Z, et al.: Crystal structure, bond characteristics, and microwave dielectric properties of novel low-εr LiRE(PO3)4 (RE = pr, Nd) ceramics, Ceram. Int., 51, [4], 5249 – 5261, (2025). doi: https://doi.org/10.1016/j.ceramint.2024.11.499

10 Li, J., Liu, P., Fu, Z.F. et al.: Microwave dielectric properties of low-fired Mg1.9Cu0.1SiO4-(La0.5Na0.5)TiO3 composite ceramics, J. Alloy. Compd., 660, 93 – 98, (2015). doi: https://doi.org/10.1016/j.jallcom.2015.11.110

11 Kim, J.S., Song, M.E., Joung, M.R., Choi, J.H., Nahm, S., Gu, S.I., Choi, B.H.: Effect of B2O3 addition on the sintering temperature and microwave dielectric properties of Zn2SiO4 ceramics, J. Eur. Ceram Soc., 30, [2], 375 – 379, (2010). doi: https://doi.org/10.1016/j.jeurceramsoc.2009.04.028

12 Wee, S.H., et al.: Low-temperature sintering of V2O5-added and -substituted ZnNb2O6 microwave ceramics, Jpn. J. Appl. Phys., 43, [6A], 3511, (2004). doi: https://doi.org/10.1143/JJAP.43.3511

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH