Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Comparison of the Composition and Pore Structure of Four Common Zisha from Yixing City after Firing

J. Wang1, X. Zhu2

1 School of Fine Arts, Suzhou Vocational University, Suzhou, Jiangsu 215104, China.
2 School of Mechano-Electronic Engineering, Suzhou Vocational University, Suzhou, Jiangsu 215104, China.

received November 26, 2024, received in revised form February 18, 2025, accepted February 20, 2025

Vol. 16, No. 2, Pages 77-84   DOI: 10.4416/JCST2024-00031

Abstract

Zisha teapots are the most famous among the multitude of types of pottery made in China. The high porosity of Zisha teapots may be the reason for their perfect effect in tea brewing. However, there are many types of Zisha (including purple clay, red clay, and Duan clay), and their chemical composition, phase composition and pore structure may also vary. Here, we investigated the relationship between the composition and pore structure of four types of Zisha. The pore distribution of Qingshuini Zisha (QSN-ZS) and Qinghui-Duan Zisha (QHD-ZS) in the range of 0.02 – 3 μm far exceeds that of the other two Zisha. Meanwhile, QSN-ZS and QHD-ZS also have higher porosity. The porosity is related to the content of Fe2O3, and a medium content (2.5 wt% – 5 wt%) of Fe2O3 is beneficial for high porosity.

Download Full Article (PDF)

Keywords

Zisha, composition, pore structure, hematite.

References

1 Wu, X., Zhang, C., Goldberg, P., Cohen, D., Pan, Y., Arpin, T., Bar-Yosef, O.:Early Pottery at 20,000 Years Ago in Xianrendong Cave, China, Science, 336, 1696 – 1700, (2012).

2 Lee, V., Attinger, D.: Thermodynamics and historical relevance of a jetting thermometer made of chinese zisha ceramic, Scientific Reports, 6, 28609, (2016).

3 Gowlland, G.: Style, skill and modernity in the zisha pottery of china, J. Mod. Craft, 2, 129 – 142, (2009).

4 Zhu, J., MacDonald, B.L., Hang, T., Zhu, Z., Glascock, M.D.: Compositional characterization of zisha clay from the yixing area (Jiangsu, China) by neutron activation analysis, Microchem. J., 147, 1117 – 1122, (2019).

5 Gao, X., Hein, A., Quinn, P.: Tea for Two: the dual modes of contemporary zisha teaware production and their implications for archaeological research, Ethnoarchaeology, 15, 87 – 109, (2023).

6 Jiang, H.: Tea as nature, tea as power in early modern China: tea and the literati in the ming dynasty, Asian Hist. Cul., 15, 1 – 10, (2023).

7 Liao, Z.H., Chen, Y.J., Tzen, J.T.C., Kuo, P.C., Lee, M.R., Mai, F.D., Rairate, T., Chou, C.C.: Effect of teapot materials on the chemical compositions of oolong tea infusion, J. Sci. Food Agr., 98, 751 – 757, (2018).

8 Chung, T.Y., Kuo, P.C., Liao, Z.H., Shih, Y.E., Yang, M.L., Cheng, M.L., Wu, C.C., Tzen, J.T.C.: Analysis of lipophilic compounds of tea coated on the surface of clay teapots, J. Food Drug. Anal., 23, 71 – 81, (2015).

9 Wu, J., Hou, T., Zhang, M., Li, Q., Wu, J., Li, J., Deng, Z.: An analysis of the chemical composition, performance and structure of china yixing zisha pottery from 1573 A.D. to 1911 A.D., Ceram. Int., 39, 2589 – 2595, (2013).

10 Lin, Y., Hu, C., Ding, D., Hang, H., Yang, C., Li, Y., Shen, Y.: The compositions and pore structures of benshanzhu zisha ceramics, J. Ceram. Sci. Technol., 12, 107 – 114, (2021).

11 Yang, C., Kong, J., Yang, J., Chu, C., Wang, X., Li, Y.: The study of crystal-phase composition and pore structure for dicaoqing-zisha compared with porcelain and pottery, Ceram. Int., 47, 10650 – 10657, (2021).

12 Vega-Mendoza, M.S., Luévano-Hipólito, E., Torres-Martínez, L.M.: Design and fabrication of photocatalytic coatings with α/β-Bi2O3 and recycled-fly ash for environmental remediation and solar fuel generation, Ceram. Int., 47, 26907 – 26918, (2021).

13 Hu, L., Zhao, D., Liu, C., Liang, Y., Zheng, D., Sun, S., Li, Q., Liu, Q., Luo, Y., Liao, Y., Xie, L., Sun, X.: Amorphous CoB nanoarray as a high-efficiency electrocatalyst for nitrite reduction to ammonia, Inorg. Chem. Front., 23, 6075 – 6079, (2022).

14 Cao, G., Wang, X., Hu, J., Qu, J., Sun, W., Li, C. M., Yang, X.: Charge reaction kinetics on TiO2 nanotubes under photoelectrochemical water oxidation condition, Appl. Surf. Sci., 603, 154447, (2022).

15 Tharani, K., Christy, A. J., Sagadevan, S., Nehru, L. C.,: Photocatalytic and antibacterial performance of iron oxide nanoparticles formed by the combustion method, Chem. Phys. Lett., 771, 138524, (2021).

16 Toby, B.H., Von Dreele, R.B.: GSAS-II: the genesis of a modern open-source all purpose crystallography software package, J. Appl. Crystallogr., 46, 544 – 549, (2013).

17 Bernasconi, A., Pellegrino, L., Vergani, F., Campanale, F., Marian, N.M., Galimberti, L., Perotti, M., Viti, C., Capitani, G.: Recycling detoxified cement asbestos slates in the production of ceramic sanitary wares, Ceram. Int., 49, 1836 – 1845, (2023).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH