Design of an Automatic Grinding Machine for the Bottom of Ceramic Plates based on TRIZ Theory
S. Zhang1, X. Gao2, Q. Chen1, Y. Qi1, M. Lei1
1 Institute of Intelligent Manufacturing and Smart Transportation, Suzhou City University, Suzhou, 215104 China
2 Department of Electromechanical Engineering, Tangshan University, Tangshan, 063000, China
received March 3, 2024, received in revised form March 25, 2024, accepted March 28, 2024
Vol. 15, No. 1, Pages 29-36 DOI:
Abstract
To address the issue of high labor intensity and potential hand injury associated with manual grinding of the bottom of ceramic plates, an automatic bottom grinding machine for ceramic plates was designed using the TRIZ theory product design process.
Keywords
TRIZ theory, contradiction matrix, physical field analysis, ceramic plate, bottom grinding machine