Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Effects of Aging Time on Microstructure, Hydrophobic and Optical Properties of BiFeO3 Thin Films Synthesized via Sol-Gel Method

H. Baqiah1, Z.A. Talib1, A.H. Shaari1, M. M. Awang Kechik1, J.Y.C. Liew1, N.B. Ibrahim2

1 Physics Department, Faculty of Science, Universiti Putra Malaysia, 43400 UPM, Serdang, Selangor, Malaysia
2 School of Applied Physics, Faculty of Science and Technology, Universiti Kebangsaan Malaysia, 43600 Bangi, Selangor, Malaysia

received May 28, 2018, received in revised form June 26, 2018, accepted June 26, 2018

Vol. 9, No. 4, Pages 419-426   DOI: 10.4416/JCST2018-00039

Abstract

BiFeO3 (BFO) films were synthesized with the sol-gel method followed by the spin coating technique using 2-methoxyethanol as solvent and acetylacetone as chelating agent. The effects of aging time (t = 0, 1, 3, 6 days) of the BFO sol on the microstructure, wettability and optical properties of BFO films were investigated by means of X-ray diffraction (XRD), atomic force microscopy (AFM), contact angle (CA) measurement, Uv-vis and photoluminescence. The crystallinity of films was affected by t. Crystallite size of the films changed slightly in the range of 14.2 – 15.2 nm while the lattice parameters clearly varied with t. The average particle size of BFO films ranged between 45.9 and 52.7 nm while the mean square roughness (Rq) varied between 1.0 and 4.2 nm. The films showed maximum optical transmittance (81 – 90 %) in the range 600 – 800 nm. The band gap of the films was also affected with t, and it has a value of 2.85 to 2.76 eV. The films showed a hydrophobic property with CA ranging between 95.3 to 104.7 °. The best crystallinity, lowest Rq and highest Eg = 2.85 eV were obtained for the film with t = 1 day. The results demonstrate possible development of a superhydrophobic coating using BiFeO3 coating.

Download Full Article (PDF)

Keywords

BiFeO3 films, wettability, aging time, roughness, band gap

References

1 Catalan, G., Scott, J.F.: Physics and applications of bismuth ferrite, Adv. Mater., 21, 2463 – 2485, (2009).

2 Wu, J., Fan, Z., Xiao, D., Zhu, J., Wang, J.: Multiferroic bismuth ferrite-based materials for multifunctional applications: ceramic bulks, thin films and nanostructures, Prog. Mater. Sci., 84, 335 – 402, (2016).

3 Kumari, C., Varun, I., Tiwari, S.P., Dixit, A.:. Robust non-volatile bipolar resistive switching in sol-gel derived BiFeO3 thin films, Superlattices Microstruct., 120, 67 – 74, (2018).

4 Satar, N.S.A., Aziz, A.W., Yaakob, M.K., Yahya, M.Z.A., Hassan, O.H., Kudin, T.I.T., Kaus, N.H.M.: Experimental and first-principles investigations of lattice strain effect on electronic and optical properties of biotemplated BiFeO3 nanoparticles, J. Phys. Chem. C., 120, 26012 – 26020, (2016).

5 Bai, X., Wei, J., Tian, B., Liu, Y., Reiss, T., Guiblin, N., Gemeiner, P., Dkhil, B., C. Infante, I.: Size effect on optical and photocatalytic properties in BiFeO3 nanoparticles, J. Phys. Chem. C., 120, 3595 – 3601, (2016).

6 Li, S., Lin, Y.H., Zhang, B.P., Wang, Y., Nan, C.W.: Controlled fabrication of BiFeO3 uniform microcrystals and their magnetic and photocatalytic behaviors, J. Phys. Chem. C., 114, 2903 – 2908, (2010).

7 Li, Z., Shen, Y., Yang, C., Lei, Y., Guan, Y., Lin, P.Y.H., Liu, D., Nan, C.: Significant enhancement in the visible light photocatalytic properties of BiFeO3-graphene nanohybrids, J. Mater. Chem. A., 823 – 829, (2013).

8 Bao, X.-M., Cui, J.-F., Sun, H.-X., Liang, W.-D., Zhu, Z.-Q., An, J., Yang, B.-P., La, P.-Q., Li, A.: Facile preparation of superhydrophobic surfaces based on metal oxide nanoparticles, Appl. Surf. Sci., 303, 473 – 480, (2014).

9 Pahari, D., Das, N.S., Das, B., Chattopadhyay, K.K., Banerjee, D.: Tailoring the optical and hydrophobic property of zinc oxide nanorod by coating with amorphous graphene, Phys. E Low-dimensional Syst. Nanostructures, 83, 47 – 55, (2016).

10 Dave, V., Gupta, H.O., Chandra, R.: Nanostructured hydrophobic DC sputtered inorganic oxide coating for outdoor glass insulators, Appl. Surf. Sci., 295, 231 – 239, (2014).

11 Lin, S.-S., Liao, C.-S.: The hydrophobicity and optical properties of the HfO2-deposited glass, Ceram. Int., 39, 353 – 358, (2013).

12 Azimi, G., Dhiman, R., Kwon, H.M., Paxson, A.T., Varanasi, K.K.: Hydrophobicity of rare-earth oxide ceramics, Nat. Mater., 12, 315 – 320, (2013).

13 Martínez-González, R., Estelrich, J., Busquets, M.A.: Liposomes loaded with hydrophobic iron oxide nanoparticles: suitable T2 contrast agents for MRI, Int. J. Mol. Sci., 17, 1209, (2016).

14 Cao, L., Lu, X., Pu, F., Yin, X., Xia, Y., Huang, W., Li, Z.: Facile fabrication of superhydrophobic Bi/Bi2O3 surfaces with hierarchical micro-nanostructures by electroless deposition or electrodeposition, Appl. Surf. Sci., 288, 558 – 563, (2014).

15 Martin, L.W., Chu, Y.-H., Ramesh, R.: Advances in the growth and characterization of magnetic, ferroelectric, and multiferroic oxide thin films, Mater. Sci. Eng. R Reports, 68, 89 – 133, (2010).

16 Baqiah, H., Ibrahim, N.B., Halim, S.A., Flaifel, M.H., Abdi, M.H.: The role of cobalt doping on magnetic and optical properties of indium oxide nanostructured thin film prepared by sol-gel method, Mater. Res. Bull., 63, 147 – 154, (2015).

17 Baqiah., H., Ibrahim., N.B., Abdi, M.H., Halim., S.A.: Electrical transport, microstructure and optical properties of Cr-doped In2O3 thin film prepared by sol-gel method, J. Alloy. Compd., 575, 198 – 206, (2013).

18 Dong, G., Tan, G., Liu, W., Xia, A., Ren, H.: Effect of tb doping on structural and electrical properties of BiFeO3 thin films prepared by Sol-Gel technique, J. Mater. Sci. Technol., 30, 365 – 370, (2014).

19 Hong, D., Yu, S., Cheng, J.: Sm-Ti co-substituted BiFeO3 thin films prepared by sol-gel technique, Curr. Appl. Phys., 11, S255 – S259, (2011).

20 Sharma, S., Saravanan, P., Pandey, O.P., Vinod, V.T.P., Černík, M., Sharma, P.: Magnetic behaviour of sol-gel driven BiFeO3 thin films with different grain size distribution, J. Magn. Magn. Mater., 401, 180 – 187, (2016).

21 Shirahata, Y., Oku, T.: Characterization and photovoltaic properties of BiFeO3 thin films, Coatings, 6, 68, (2016).

22 Soram, B.S., Ngangom, B.S., Sharma, H.B.: Effect of annealing temperatures on the structural and optical properties of sol-gel processed nanocrystalline BiFeO3 thin films, Thin Solid Films, 524, 57 – 61, (2012).

23 Ibrahim, N.B., Al-Shomar, S.M., Ahmad, S.H.: Effect of aging time on the optical, structural and photoluminescence properties of nanocrystalline ZnO films prepared by a sol-gel method, Appl. Surf. Sci., 283, 599 – 602, (2013).

24 Fu, Q., Cao, C.-B., Zhu, H.-S.: Preparation of alumina films from a new sol-gel route. Thin Solid Films, 348, 99 – 102, (1999).

25 Go, R., López, R., Gómez, R.: Band-gap energy estimation from diffuse reflectance measurements on sol – gel and commercial TiO2: A comparative study, J. Sol-Gel Sci. Technol., 61, 1 – 7, (2012).

26 Hauser, A.J., Zhang, J., Mier, L., Ricciardo, R.A., Woodward, P.M., Gustafson, T.L., Brillson, L.J., Yang, F.Y.: Characterization of electronic structure and defect states of thin epitaxial BiFeO3 films by UV-visible absorption and cathodoluminescence spectroscopies, Appl. Phys. Lett., 92, 222901 (2008).

27 Chen, X., Zhang, H., Wang, T., Wang, F., Shi, W.: Optical and photoluminescence properties of BiFeO3 thin films grown on ITO-coated glass substrates by chemical solution deposition, Phys. status solidi., 209, 1456 – 1460, (2012).

28 Xu, J.-P., Zhang, R.-J., Chen, Z.-H., Wang, Z.-Y., Zhang, F., Yu, X., Jiang, A.-Q., Zheng, Y.-X., Wang, S.-Y., Chen, L.-Y.: Optical properties of epitaxial BiFeO3 thin film grown on SrRuO3-buffered SrTiO3 substrate, Nanoscale Res. Lett., 9, 188, (2014).

29 Liu, H.L., Lin, M.K., Cai, Y.R., Tung, C.K., Chu, Y.H.: Strain modulated optical properties in BiFeO3 thin films, Appl. Phys. Lett., 103, 181907, (2013).

30 Mishra, D.K., Qi, X.: Energy levels and photoluminescence properties of nickel-doped bismuth ferrite, J. Alloy. Compd., 504, 27 – 31, (2010).

31 Singh, A., Khan, Z.R., Vilarinho, P.M., Gupta, V., Katiyar, R.S.: Influence of thickness on optical and structural properties of BiFeO3 thin films: PLD grown, Mater. Res. Bull., 49, 531 – 536 (2014).

32 Ramachandran, B., Dixit, A., Naik, R., Lawes, G., Rao, M.S.R.: Charge transfer and electronic transitions in polycrystalline BiFeO3, Phys. Rev. B., 82, 012102, (2010).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources