Journal of Ceramic Science and Technology

The Journal of Ceramic Science and Technology publishes original scientific articles on all topics of ceramic science and technology from all ceramic branches. The focus is on the scientific exploration of  the relationships between processing, microstructure and properties of sintered ceramic materials as well as on new processing routes for innovative ceramic materials. The papers may have either theoretical or experimental background. A high quality of publications will be guaranteed by a thorough double blind peer review process.

The Journal is published by Göller Verlag GmbH on behalf of the Deutsche Keramische Gesellschaft (DKG). Edited by Yu-Ping Zeng, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China.

  • Home
  • Early view
  • Articles
    • All articles
    • Recent Articles
    • Early Views
  • Issues
  • Submit an article
  • Guidelines for Referees
  • Guidelines for Authors
  • Open Access
  • Editorial Board
  • Copyright
  • Order journal / article
  • Customer area
  • Terms of Service

Journal Metrics

Web of science
Impact Factor: 1,220
Impact Factor without Journal Self Cites: 1,060
5 Year Impact Factor: 0,818

Scopus
Scimago Journal Rank (SJR):  0,378

 

Prices

Authors
1,300 € Open Access

Print Subscription
62 € per year

view all subscriptions

 

Payment methods

 Credit card

 Invoice

 Wire transfer

 

Articles

All articles  |  Recent articles

Effect of Submicron-Carbon-Containing MgO-C Refractories on Carbon Pickup of Ultra-Low Carbon Steel

Y. Liu1,2, L. Wang2, G. Li1,2,3, Z. Zhang2, X. Xu1, Y. Li1, J. Chen1

1 The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China
2 Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, China
3 Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing, Beijing, 100083, China

received October 30, 2017, received in revised form December 19, 2017, accepted January 29, 2018

Vol. 9, No. 2, Pages 141-148   DOI: 10.4416/JCST2017-00087

Abstract

To reduce the carbon pickup of ultralow-carbon steel, the interaction between liquid steel and MgO-C refractories containing submicron carbon at 1600 °C was studied under laboratory conditions and compared with interaction of liquid steel with conventional MgO-C refractories containing flaky graphite. The results show that the carbon pickup in steel is provided by the spalling refractories, the penetration layer and the reaction of Al in steel with CO, which is generated from the reaction between MgO and C in refractories. The carbon supplied by spalling refractories might play a dominant role in the carbon pickup of steel. The reaction between Al in steel and CO is not the main cause of carbon pickup. In the test with conventional MgO-C refractories, carbon pickup became more severe with increasing content of flaky graphite. In the test with MgO-C refractories containing submicron carbon, the carbon pickup decreased with increasing submicron-carbon content, which is attributed to the thinner penetration layer and better spalling resistance. The application of MgO-C refractories containing submicron carbon could be favourable for the manufacture of ultralow-carbon steel with high cleanliness.

Download Full Article (PDF)

Keywords

Submicron carbon, MgO-C refractories, carbon pickup, penetration, spalling resistance

References

1 Cooper, C.F., Alexander, I.C., Hampson, C.J.: The role of graphite in the thermal shock resistance of refractories, Br. Ceram. Trans. J., 84, 57 – 62, (1985).

2 Liang, F., Li, N., Liu, B., He, Z.: Processing and characterization of multi-walled carbon nanotubes containing alumina-carbon refractories prepared by nanocomposite powder technology, Metall. Mater. Trans. B, 47, 1661 – 1668, (2016).

3 Benedetti, B.D.E.: The resin union magnesium carbon brick bears corrosiveness, Br. Ceram. Trans. J., 3, 55 – 57, (1989).

4 Chen, J., Li, N., Yan, W.: Influence of Ti3AlC2 on corrosion resistance and microstructure of Al2O3-Ti3AlC2-C refractories in contact with ladle slag, J. Eur. Ceram. Soc., 36, 1505 – 1511, (2016).

5 Faghihi-Sani, M.A., Yamaguchi, A.: Oxidation kinetics of MgO-C refractory bricks, Ceram. Int., 28, 835 – 839, (2002).

6 Sasai, K., Mizukami, Y.: Reaction rate between alumina graphite immersion nozzle and low carbon steel, ISIJ Int., 35, 26 – 33, (1995).

7 Ruan, G.Z., Li, N.: Carbon pickup of interstitial free steel from Al2O3-C refractories, Ironmak. Steelmak., 31, 342 – 344, (2004).

8 Jansson, S., Brabie, V., Jönsson, P.: Magnesia-carbon refractory dissolution in al killed low carbon steel, Ironmak. Steelmak., 33, 389 – 397, (2006).

9 Zhao, L., Sahajwalla, V.: Interfacial phenomena during wetting of graphite/alumina mixtures by liquid iron, ISIJ Int., 43, 1 – 6, (2003).

10 Lee, J., Tazuke, A., Tanaka, T., Park, J.H.: Estimation of sulfur segregation at the interface between molten iron and graphite substrate from wetting experiments, Met. Mater. Int., 15, 501 – 505, (2009).

11 Pickering, G.D., Batchelor, J.D.: Carbon-MgO reactions in BOF refractories, Am. Ceram. Soc. Bull., 50, 611 – 614, (1971).

12 Robinson, P.C.: Some observation on unused and used refractories from oxygen steelmaking vessels, Refract. J., 42, 218 – 222, (1966).

13 Kim, S.M., Lu, W.K.: Kinetics and mechanism of the formation of dense MgO layer in pitch-bearing magnesite brick during service, Metall. Trans. B, 9, 353 – 364, (1978).

14 Watanabe, A., Takahashi, H., Nakatani, F.: Mechanism of dense magnesia layer formation near the surface of magnesia-carbon brick, J. Am. Ceram. Soc., 69, 213 – 214, (1986).

15 Brabie, V.: A study on the mechanism of reaction between refractory materials and aluminium deoxidised molten steel, Steel Res. Int., 68, 54 – 60, (1997).

16 Zhu, T., Li, Y., Sang, S., Jin, S., Wang, H.: Formation of hollow MgO – rich spinel whiskers in low carbon MgO-C refractories with al additives, J. Eur. Ceram. Soc., 34, 4425 – 4432, (2014).

17 Hashemi, B., Nemati, Z.A., Faghihi-Sani, M.A.: Effects of resin and graphite content on density and oxidation behavior of MgO-C refractory bricks, Ceram. Int., 32, 313 – 319, (2006).

18 Gokce, A.S., Gurcan, C., Ozgen, S., Aydin, S.: The effect of antioxidants on the oxidation behaviour of magnesia-carbon refractory bricks, Ceram. Int., 34, 323 – 330, (2008).

19 Bag, M., Adak, S., Sarkar, R.: Study on low carbon containing MgO-C refractory: Use of nano carbon, Ceram. Int., 38, 2339 – 2346, (2012).

20 Bag, M., Adak, S., Sarkar, R.: Nano carbon containing MgO-C refractory: Effect of graphite content, Ceram. Int., 38, 4909 – 4914, (2012).

21 Ochiai, T.: Development of refractories by applying nano-technology, Refractories (Tokyo), 56, 152 – 159, (2004).

22 Xuejun, Y., Zheming, Q., Liangquan, H.: The influence of nanometer carbon black on the mechanical properties of phenolic resin, Process. Aircraft. Mater., 33, 34 – 38, (2003).

23 Xianhui, L., Chifei, W.: The optimization of characterization and preparation on nanometer carbon blacks, Process. Technol. Nano. Mater., 2, 47 – 49, (2005).

24 Takanaga, S., Fujiwara, Y., Hatta, M.: Nano – Tech. refractories 3: Development of MgO-rimmed MgO-C brick. In: Proceedings of the 9th UNITCER-2005. Orlando, FL, USA, 2005.

25 Wei, Y., Li, N., Ke, C.: Effect of silicon carbide on reactions between molten steel and fused magnesia-silicon carbide composite refractory, Am. Ceram. Soc. Bull., 86, 9201 – 9205, (2007).

26 Li, X., Rigaud, M., Palco, S.: Oxidation kinetics of graphite phase in magnesia-carbon refractories, J. Am. Ceram. Soc., 78, 965 – 971, (1995).

27 Xiaoqiang, S., Lin, L, Xiaoyan, P.: Effects of nanometer carbon black on the mechanical properties and thermal shock resistance of MgO-C bricks, in chinese, China Metallurgy, 6, 17 – 20, (2015).

Copyright

Göller Verlag GmbH

Special and Topcial Issues

Special Issue, 3/2025
Guest Editors:
Olaf Krause and Christian Dannert
Advances in Refractories

Topical Issue, 3/2017
Guest Editors:
Waltraud M. Kriven and Gregor J. G. Gluth
Geopolymers

Special Issue, 1/2017
Guest Editor:
Alexander Michaelis
6th International Congress on Ceramics (ICC6)

Topical Issue, 2/2016
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advan-ced steel technologies; A challenge for refractory materials and systems.

Topcial Issue, 4/2015
Low Temperature Co-fired Ceramics - LTCC

Topcial Issue, 2/2015
Status of Additive Manufacturing with Ceramics

Topical Focus, 4/2014
Materials Processing Science with Lasers as Energy Sources

Topical Issue, 2/2014
Guest Editor:
Christos Aneziris
Low carbon and carbon-free refractory approaches for advanced steel technologies; A challenge for refractory materials and systems.

Special Issue, 2/2013
Guest Editor:
Alexander Michaelis
Ceramic Materials and Components for Energy and Environmental Applications

Topical Issue, 1/2013
Ceramic Processing Science with Lasers as Energy Sources

Printed version

jcst 2015 02 cover

Order journal subscription
 

© 2009-2025 Göller Verlag GmbH