Articles
All articles | Recent articles
Low-Temperature Spark Plasma Sintering of a SiC Nanopowder with a Very Thin Al-Based Layer
K. Shimoda
Research Center for Structural Materials, National Institute for Materials Science, 1-2-1, Sengen, Tsukuba, 305 – 0047 Ibaraki, Japan.
received April 16, 2018, received in revised form May 23, 2018, accepted Juni 14, 2018
Vol. 9, No. 4, Pages 411-418 DOI: 10.4416/JCST2018-00035
Abstract
A SiC nanopowder with an Al-based layer synthesized by means of laser pyrolysis was used to fabricate bulk SiC using spark plasma sintering (SPS) at 1600 – 1800 °C. The surface structure of the novel SiC nanopowder was analyzed by means of field-emission scanning/transmission electron microscopy (FE-SEM/TEM), while the surface chemistry was characterized using X-ray photoelectron spectroscopy (XPS) and energy-dispersive X-ray spectroscopy (EDS). The average particle size was around 45 nm with a very thin (< 5 nm) coating of Al-containing compounds. The effect of the SPS temperature on the density and mechanical and thermal properties of bulk SiC was investigated. Sintered densities above 96 % were obtained at temperatures as low as 1700 °C. Toughened microstructures, which consisted of platelets and relatively small equiaxed SiC grains incorporating crystalline Al4O4C, were observed after SPS treatment at 1800 °C. The samples fabricated by means of SPS at 1800 °C had a typical bending strength of 592 MPa, fracture toughness of 5.4 MPam1/2, and thermal conductivity of 80 W/mK.
Download Full Article (PDF)
Keywords
SiC, nanopowders, additives, sintering, microstructure
References
1 Nakamura, K., Maeda, K.: Silicon Carbide Ceramics, Vol. 2, Elsevier, Barking, 1991.
2 Dapkunas, S.J.: Ceramic heat exchangers, Am. Ceram. Soc. Bull., 67, 388 – 391, (1988).
3 Willinder, M., Friesel, M., Qamar-ul, W., Straumal, B.: Silicon carbide and diamond for high temperature device applications, J. Mater. Sci., 17, 1 – 25, (2006).
4 Haris, G.L.: Properties of Silicon Carbide. G.L. Haris (Ed.), INSPEC, London, 1995.
5 Prochazka, S., Scanlan, R.M.: Effect of boron and carbon on sintering of SiC, J. Am. Ceram. Soc., 58, 72, (1975).
6 Zhou, Y., Tanaka, H., Otani, S., Bando, Y.: Low-temperature pressureless sintering of α-SiC with Al4C3-B4C-C additions, J. Am. Ceram. Soc., 82, 1959 – 1964, (1999).
7 Ghosh, A., Jenkins, M.G., White, K.W., Kobayashi, A.S., Brad, R.C.: Elevated-temperature fracture resistance of a sintered alpha-silicon carbide, J. Am. Ceram. Soc., 72, 242 – 247, (1989).
8 Nadeau, J.S.: Very high pressure hot pressing of silicon carbide, J. Am. Ceram. Soc. Bull., 52 170 – 174, (1973).
9 Xie, M.L., Luo, D.L., Xian, X.B., Leng, B.Y., Chen, C., Lu, W.Y.: Densification of nano-SiC by ultra-high-pressure effect of time, temperature and pressure, Fusion Eng. Des., 85, 964 – 968, (2010).
10 Yamamoto, T., Kitaura, H., Kodera, Y., Ishii, T., Ohyanagi, M., Munir, Z.A., Consolidation of nanostructure β-SiC by spark plasma sintering, J. Am. Ceram. Soc., 87, 1436 – 1441, (2004).
11 Maitre, A., Vande Put, A., Laval, J.P., Valette, S., Trolliard, G.: Role of boron on the spark plasma sintering of an α-SiC powder, J. Eur. Ceram. Soc., 28, 1881 – 1890, (2008).
12 Munir, Z.A., Anselmi-Tamburini, U., Ohyanagi, M.: The effect of electric field and pressure on the synthesis and consolidation of materials: A review of the spark plasma sintering method, J. Mater. Sci., 41, 763 – 777, (2006).
13 Kijima, K., Noguchi, H., Konishi, M.: Sintering of ultrafine SiC powders prepared by plasma CVD, J. Mater. Sci., 24, 2929 – 2933, (1989).
14 Kim, Y.W., Lee, Y.I., Mitomo, M.: Sinterability of nano-sized silicon carbide powders, J. Ceram. Soc. Jpn., 114, 681 – 685, (2006).
15 Shimoda, K., Park, J.S., Hinoki, T., Kohyama, A.: Densification mechanism and microstructural evolutions of SiC matrix in NITE process, Ceram. Eng. Sci. Proc., 27, 19 – 27, (2006).
16 Malinge, A., Coupe, A., Petitcorps, Y.L., Pailler, R.: Pressureless sintering of beta silicon carbide nanoparticles, J. Eur. Ceram. Soc., 32, 4393 – 4400, (2012).
17 Shimoda, K., Park, J.S., Hinoki, T., Kohyama, A.: Influence of surface structure of SiC nano-sized powder analyzed by X-ray photoelectron spectroscopy on basic powder characteristics, Appl. Surf. Sci., 253, 9450 – 9456, (2007).
18 Shimoda, K., Koyanagi, T.: Surface properties and dispersion behaviors of SiC nanopowders, Colloid. Surf. A., 463, 93 – 100, (2014).
19 Raju, K., Yoon, D.H.: Sintering additives for SiC based on the reactivity: A review, J. Ceram. Int., 42, 17947 – 17962, (2016).
20 Omori, M., Takei, H.: Pressureless sintering of SiC, J. Am. Ceram. Soc., 65, C92 – C96, (1982).
21 Noviyanto, A., Yoon, D.H.: Rare-earth oxide additives for the sintering of silicon carbide, Diam. Relat. Mater., 38, 124 – 130, (2013).
22 Taguchi, S.P., Motta, F.V., Balestra, R.M., Riberio, S.: Wetting behavior of SiC ceramics. Part II-Y2O3/Al2O3 and Sm2O3/Al2O3, Mater. Lett., 58, 2810 – 2814, (2004).
23 Shimoda, K., Kondo, S., Hinoki, T., Kohyama, A.: Thermal stress relaxation creep and microstructural evolutions of nanostructured SiC ceramics by liquid phase sintering, J. Eur. Ceram. Soc., 30, 2643 – 2652, (2010).
24 Parker, W.J., Jenkins, R.J., Butler, C.P., Abbott, G.L.: Flash method of determining thermal diffusivity, heat capacity, and thermal conductivity, J. Appl. Phys., 32, 1679 – 1684, (1961).
25 Strohmeier, B.R.: An ESCA method for determining the oxide thickness on aluminum alloys, Surf. Interface. Anal., 15, 51 – 56, (1990).
26 Lee, C.W., Pineau, F.J., Corelli, J.C.: Thermal properties of neutron-irradiated SiC; effects of boron doping, J. Nucl. Mater., 108, 678 – 684, (1982).
27 Tamari, N., Tanaka, T., Tanaka, K., Kondoh, I., Kawahara, M., Tokita, M.: Effect of spark plasma sintering on densification and mechanical properties of silicon carbide, J. Ceram. Soc. Jpn., 103, 740 – 742, (1995).
28 Levin, E.M., Robbins, C.R., McMurdie, H.E.: Phase diagrams for ceramists, The American Ceramic Society, Inc., 1969, pp. 165.
29 Xu, H., Bahtia, T., Deshpande, S.A., Padture, N.P., Ortiz, A.L., Cumbrera, F.L.: Microstructural evolution in liquid-phase-sintered SiC: part I, effect of starting powder, J. Am. Ceram. Soc., 84, 1578 – 584, (2001)
30 Ragaru, C., Lancin, M., Marhic, C.: β→α phase transformation in SiC: link between polytypism, dihedral angle and nucleation mechanism of α twins, J. Eur. Ceram. Soc., 19, 2701 – 2709, (1999).
31 Zawrah, M.F., Shaw, L.: Liquid-phase sintering of SiC in presence of CaO, Ceram. Int., 30, 721 – 725, (2004).
32 Gomez, E., Echeberria, J., Iturriza, I., Castro, F.: Liquid phase sintering of SiC with additions of Y2O3, Al2O3 and SiO2, J. Eur. Ceram. Soc., 24, 2895 – 2903, (2004).
33 Kim, Y.W., Mitomo, M., Emoto, H., Lee, J.G.: Effect of initial α-phase on microstructure and mechanical properties of sintered silicon carbide, J. Am. Ceram. Soc., 81, 3136 – 3140, (1998).
34 Lee, J.K., Park, J.G., Lee, E.G., Seo, D.S., Hwang, Y.: Effect of starting phase on microstructure and fracture toughness of hot-pressed silicon carbide, Mater. Lett., 57, 203 – 208, (2002).
35 Slack, G.A.: Thermal conductivity of pure and impure silicon, silicon carbide, and diamond, J. Appl. Phys., 35, 3460 – 3466, (1964).
36 Cho, T.Y., Kim, Y.W.: Effect of grain growth on the thermal conductivity of liquid-phase sintered silicon carbide ceramics, J. Eur. Ceram. Soc., 37, 3475 – 3481, (2017).
37 Sakai, T., Aikawa, T.: Phase transformation and thermal conductivity of hot-pressed silicon carbide containing alumina and carbon, J. Am. Ceram. Soc., 71, C-7-C-9, (1988).
38 Foster, L.M., Long, G., Hunter, M.S., Reactions between aluminum oxide and carbon the Al2O3-Al4C3 phase diagram, J. Am. Ceram. Soc., 39, 1 – 11, (1956).
39 Zhao, J., Lin, W., Yamaguchi, A.: Influence of heating temperature, keeping time and raw materials grain size on Al4O4C synthesis in carbothermal reduction process and oxidation of Al4O4C, J. Ceram. Soc. Jpn., 115, 654 – 660, (2007).
Copyright
Göller Verlag GmbH