Articles
All articles | Recent articles
Corrigendum to “Relationship of Optical Properties and Elastoplastic Characteristics of Transparent Spark-Plasma-Sintered YSZ Ceramics” [J. Ceram. Sci. Technol. 08 [01] 161-168 (2017)]
O. L. Khasanov, E. S. Dvilis, Z. G. Bikbaeva, V. D. Paygin, A. O. Khasanov
Department of Nanomaterials and Nanotechnologies, National Research Tomsk Polytechnic University, Tomsk, Russia-634050
received October 31, 2016, received in revised form December 31, 2016, accepted January 21, 2017
Vol. 8, No. 2, Pages 305-306 DOI: 10.4416/JCST2016-00105-CORR
Abstract
DOI of the original article: 10.4416/JCST2016-000105
The autors regret that in the original published version of this article the acknowledgments part was missing. The missing part appears below:
Download Full Article (PDF)
Keywords
References
Copyright