Additive Manufacturing to Produce Complex 3D Ceramic Parts
T. Chartier1, C. Dupas1, M. Lasgorceix1, J. Brie2, 1, N. Delhote3, Chr. Chaput4
1 CNRS, Université de Limoges, SPCTS UMR 7315, Centre Européen de la Céramique, 12 rue Atlantis, 87068 Limoges, France
2 CHU de Limoges, Service de Chirurgie Maxillo-Faciale, 2 avenue Martin Luther-King, 87042 Limoges, France
3 CNRS, Université de Limoges, XLIM UMR 7252, 123 Avenue Albert Thomas, 87060 Limoges, France
4 3DCeram, 27 rue du Petit Theil, 87280 Limoges, France
received September 15, 2014, received in revised form October 17, 2014, accepted December 2, 2014
Vol. 6, No. 2, Pages 95-104 DOI: 10.4416/JCST2014-00040
Abstract
Attempts to improve the performance of ceramic parts have recently led to advances in their design and in the processes used to tailor these parts. Thus, Additive Manufacturing (AM) technologies, initially developed in the polymers and metals industries, have become of increasing interest for shaping ceramic parts. Among AM techniques, photopolymerization (referred to as stereolithography (SLA) and micro-stereolithography) makes it possible to reach high accuracy that matches the design requirements for new applications of ceramics in a wide range of fields. The development by means of (micro)-stereolithography of complex 3D ceramic parts with improved performance requires the mastering of various parameters linked to the inorganic-organic system involved in this processing route. This paper reports on some recent achievements in the production of ceramics using photopolymerization. Some examples of the work performed at the SPCTS laboratory to produce complex 3D ceramic parts for applications in the fields of information and communication technologies, healthcare and jewellery are presented.
Download Full Article (PDF)
Keywords
Shaping, additive manufacturing, photopolymerization, stereolithography
References
1 Brady, G.A., Halloran, J.W.: Stereolithography of ceramic suspensions, Rapid Prototyping J., 3, 61 – 65, (1997).
2 Griffith, M.L., Halloran, J.W.: Freeform fabrication of ceramics via stereolithography, J. Am. Ceram. Soc., 79, 2601 – 2608, (1996).
3 Jacobs, P.F.: Rapid prototyping & manufacturing: Fundamentals of stereolithography. Society of Manufacturing Engineers, Dearborn, MI, 1992.
4 Wray, P.: Additive manufacturing – turning manufacturing inside out, Am. Ceram. Soc. Bull., 93, 17 – 23, (2014).
5 Standards terminology for AM technologies - ASTM F2792 – 12a
6 Liao, H.: Stereolithography using compositions containing ceramic powders. PhD Thesis, University of Toronto, Toronto, 1997.
7 Chartier T.: Ceramic forming processes. In: Ceramic Materials, Processes, Properties and Applications. Boch, P. and Niepce J.C. Ed., ISTE Pub., London 2007.
8 Kunieda, M., Nakagawa, T.: Manufacturing of laminated deep drawing dies by laser beam cutting, Adv. Tech. Plast., 4, (1984).
9 Griffin, C., Daufenbach, J., McMillin, S.: Desktop manufacturing: LOM vs pressing, Am. Ceram. Soc. Bull., 8, 109 – 113, (1994).
10 Deckard, C.R.: Part generation by layerwise selective sintering. MS Thesis, University of Texas, Austin, Texas, 1986.
11 Deckard, C.R.: Method and apparatus for producing parts by selective sintering. US Patent 4,863,538, (1989).
12 Chartier, T., Chaput, C., Doreau, F., Loiseau M.: Stereolithography of structural complex ceramic parts, J. Mater. Sci., 37, 3141 – 3147, (2002).
13 Gibson, I., Shi, D.: Material properties and fabrication parameters in selective laser sintering, Rapid Prototyping J., 3, 129 – 136, (1997).
14 Bourrel, D.L., Marcus, H.L., Barlow, J.W., Beaman, J.J.: Selective laser sintering of metals and ceramics, Int. J. Powder Metall., 28, 369 – 381, (1992).
15 Michaels, S., Sachs, E.M., Cima, M.J.: Metal parts generation by three-dimensional printing. In: Proceedings of the Solid Freeform Fabrication Symposium. University of Texas, Austin, Texas, 1992.
16 Sachs, E., Cima, M., Cornie, J., Brancazio, D., Bredt, J., Curodeau, A., Fan, T., et al.: Micro-constructive manufacturing by three-dimensional printing. In: Proceedings of the NSF Design and Manufacturing Systems Conference, Charlotte, NC, 1993.
17 Derby, B.: Inkjet printing ceramics: from drops to solid, J. Eur. Ceram. Soc., 31, 2543 – 2550, (2011).
18 Noguera, R., Lejeune, M., Chartier, T.: 3D fine scale ceramic components formed by ink-jet prototyping process, J. Eur. Ceram. Soc., 25, 2055 – 2059 (2005).
19 Crump, S.S., Comb, J.W., Priedeman, W.R., Zinniel, R.L.: Process of support removal for fused deposition modelling. US Patent 5,503,785, (1996).
20 Chen, Z., Li, D., Lu, B., Tang, Y., Sun, M., Xu, S.: Fabrication of osteostructure analogous scaffolds via fused deposition modelling, Scripta Mater., 52, 157 – 161, (2005).
21 Lou, G.M., Cornejo, I.A., McNulty, T.F., Safari, A., Danforth, S.C.: Fabrication of piezoelectric ceramic/polymer composite transducers using fused deposition of ceramics, J. Am. Ceram. Soc., 83, 124 – 128, (2000).
22 Lasgorceix, M.: Shaping by microstereolithography and sintering of macro-micro-porous ceramics made of silicated-hydroxyapatite and biological evaluation, in French, PhD Thesis, University of Limoges, France, 2014.
23 Hull, C.W.: Apparatus for production of three-dimensional objects by stereolithography, US Patent 4,575,330, (1986).
24 Hinczewski, C., Corbel, S., Chartier, T.: Ceramic suspensions suitable for stereolithography, J. Eur. Ceram. Soc., 18, 582 – 590, (1998).
25 Hull, C.W.: Method for production of three-dimensional bodies by stereolithography. US Patent 5,174,943, (1992).
26 Halloran, J.W., Tomeckova, V., Gentry, S., Das, S., Cilino, P., et al.: Photopolymerization of powder suspension for shaping ceramics, J. Eur. Ceram. Soc., 31, 2613 – 2619, (2011).
27 Chartier, T., Badev, A., Abouliatim, Y., Lebaudy, P., Lecamp, L.: Stereolithography process: Influence of the rheology of silica suspensions and of the medium on polymerization kinetics – cured depth and width, J. Eur. Ceram. Soc., 32, 1625 – 1634, (2012).
28 Gentry, S.P., Halloran, J.W.: Absorption effect in photopolymerized ceramic suspension, J. Eur. Ceram. Soc., 33, 1989 – 1994, (2013).
29 Gentry, S.P., Halloran, J.W.: Depth and width of cured lines in photopolymerisable ceramic suspensions, J. Eur. Ceram. Soc., 33, 1981 – 1988, (2013).
30 Tomeckova, V., Halloran, J.W.: Radical depletion model for intensity effects on photopolymerization, J. Eur. Ceram. Soc., 33, 25 – 35, (2013).
31 Zhang, X., Jiang, X.N., Sun, C.: Microstereolithography of polymeric and ceramic microstructures, Sensor Actuator, 77, 149 – 156, (1999).
32 Bertsch, A., Jiguet, S., Bernhard, P., Renaud, P.: Microstereolithography: a review. In: Material Research Society Symposium Proceedings, vol. 758, Boston, Massachusetts, 2003.
33 Chartier, T., Duterte, C., Delhote, N., Baillargeat, D., Verdeyme, S., Delage, C. et al.: Fabrication of millimeter wave components via ceramic stereo- and microstereolithography processes, J. Am. Ceram. Soc., 91, 2469 – 2474, (2008).
34 Chartier, T., Badev, A.: Rapid prototyping of ceramics. In: Handbook of Advanced Ceramics: Materials, Applications, Processing and Properties. Second edition. Academic Press: Elsevier Inc., USA, 2013.
35 Badev, A., Abouliatim, Y., Chartier, T., Lebaudy, P., Lecamp, L., Chaput, C. et al.: Polymerization kinetics of a polyether acrylate in the presence of ceramic fillers used in stereolithography, J. Photoch. Photobio. A, 5, 117 – 122, (2011).
36 Wu, K.C., Halloran, J.W.: Photopolymerization monitoring of ceramic stereolithography resins by FTIR methods, J. Mater. Sci., 40, 71 – 76, (2005).
37 Delhote, N., Bila, S., Baillargeat, D., Chartier, T., Verdeyme, S.: Advanced design and fabrication of microwave components based on shape optimization and 3D ceramic stereolithography process. In: Advances in ceramics-synthesis and characterization, processing and specific applications, C. Sikalidis (Ed.), Intech, 2011.
38 Kirihara, S., Miyamoto, Y., Takenaga, K., Takeda, M.W., Kajiyama, K.: Fabrication of electromagnetic crystals with a complete diamond structure by stereolithography, Solid State Commun., 121, 435 – 439, (2002).
39 Liu, B., Gong, X., Chapell, W.J.: Applications of layer-by-layer polymer stereolithography for three-dimensional high-frequency components. In: Microwave Theory Tech., IEEE Trans, 2004.
40 Delhote, N.: Stereolithography of 3D ceramic components – microwave frequency filtering solutions, in French, PhD Thesis, University of Limoges, France, 2007.
41 Zimmermann, G., Moghaddam, A.: Allograft bone matrix versus synthetic bone graft substitutes, Injury, 42 Suppl 2, S16 – 21, (2011).
42 Chang, B.S., et al.: Osteoinduction at porous hydroxyapatite with various pore configurations, Biomaterials, 21, 1291 – 1298, (2000).
43 Bidan, C.M., Kommareddy, K.P., Rumpler, M., Kollmannsberger, P., Fratzl, P., Dunlop, J.W.C.: Geometry as a factor for tissue growth: towards shape optimization of tissue engineering scaffolds, Adv. Healthc. Mater., 2, 186 – 194, (2013).
44 Brie, J., Chartier, T., Chaput, C., Delage, C., Pradeau, B., Claire, F., et al.: A new custom made bioceramic implant for the repair of large and complex craniofacial bone defects, J. Cranio-Maxill. Surg., 41, 403 – 407, (2011).